Stucco
Relatively
New and Unpainted/To Be Stained
a.
Surface Preparation:
- if
efflorescence is present, remove by hand wire brushing; wear eye
protection and gloves; try to identify and eliminate any source
of water from behind the stucco that could have caused the efflorescence
- scrape
out and widen any cracks; brush out dust, and seal with 100% acrylic
or siliconized acrylic clear caulk; make second application in
several hours if needed; wall and chimney caps must be sound and
continuous; chimney flue should have rain cover
- treat
any mildew with a 3:1 water:household bleach mixture, leaving
it on for 20 minutes and adding more as it dries; wear eye and
skin protection; rinse thoroughly
- remove
dirt, chalk, dust, unbound sand, treated mildew, etc. by scrubbing
with detergent and water, and rinse thoroughly; or power wash
with plain water, taking care to not drive water into cracks or
porous areas
b. Priming:
- priming
is necessary to ensure maximum durability and resistance to efflorescence,
alkalinity and mildew
- use
quality exterior latex primer that is recommended for masonry
or stucco
- do
not leave a primer unstained
c. Staining:
-
use top quality exterior 100% acrylic solid color stain that is
recommended for masonry or stucco surfaces
- some
solvent based acrylic masonry or concrete stains may be applied
to stucco without priming
consult manufacturers directions
Back
|
|